Conductive foam
Specification
  • Material: irradiation cross-linked polyethylene (IXPE) foam, conductive grade
  • Resistance grade range: 10³–10⁶ Ω (conductive). The test quantity, electrode geometry, voltage and conditioning must be agreed.
  • Expansion ratio: 3–40×
  • Single-layer thickness: 0.1–15 mm
  • Laminated sections: 15–200 mm
  • Width: 500–2000 mm
  • Density: 26.8–300 kg/m³, grade-dependent
  • Forms: sheet, roll, slit strip, die-cut part, laminated sheet, adhesive-backed part
  • Colour: black or as agreed for the selected grade

IXPE conductive foam is irradiation cross-linked polyethylene foam supplied in a conductive grade. It is used where static charge must be conducted away or where two parts need a low-resistance contact path. The factory grade range is 10³–10⁶ Ω. It is not an EMI/RFI shield, and it is not a dielectric insulator. Confirm the grade, the contact face and the measurement method before approval.

Conductive versus anti-static

In this catalogue, conductive means a factory grade range of 10³–10⁶ Ω, while anti-static (dissipative) means 10⁶–10⁹ Ω. The difference is not simply “more” or “less” of the same effect. A conductive part is chosen when charge must be carried to a ground or when two conductive surfaces need a contact path. A dissipative part is chosen when the aim is to avoid charge build-up without providing a low-resistance connection.

These are supplier grade ranges, not a universal classification. A resistance reading depends on the measurement quantity (surface or volume), the electrode geometry, the applied voltage, the conditioning and the reading time. State those conditions in the purchase specification.

Contact resistance is not the material resistance alone

A conductive foam cushion is often used as a contact element. In that role, the interface matters as much as the material: contact area, compression, surface finish, oxidation, contamination and the mating material all affect the result. A low material resistance does not guarantee a low contact resistance in the assembly. Test the actual contact face and the installed compression.

Where the foam is compressed between two surfaces, define the installed compression and the compression set allowed for the service life. IXPE compression set runs from ≤2% at 3× to ≤11% at 40× under the published 23±2 °C, 22 h test. That is a material test, not a prediction of the installed joint.

Why IXPE for thin conductive parts

IXPE is cross-linked by an electron beam. The irradiation route supports a 0.1 mm single-layer thickness, a fine cell structure and a smooth surface. For a thin grounding pad, a slot liner, a tray divider or a die-cut contact cushion, those properties are useful. The base range is 3–40× expansion, 0.1–15 mm single layer, 15–200 mm heat-bonded multi-layer and 500–2000 mm width, with density from 26.8 to 300 kg/m³ depending on the ratio.

Not every IXPE sheet is conductive. The conductive grade is a selected compound and must be named on the order and on the test report. Do not infer the grade from colour alone.

What to write on the drawing or specification

ItemWhat to stateWhy it matters
Resistance quantitySurface resistance or volume resistanceThe two are different measurements and must not be substituted.
Test methodStandard, electrode geometry and specimen sizeA reading without geometry cannot be reproduced.
Applied voltageTest voltage and electrification timeThe reading is condition-dependent.
ConditioningTemperature, relative humidity and equilibration timeHumidity and temperature affect the result; agree the conditioning.
Contact faceMoulded face, cut face or laminated faceThe exposed face is the one that makes contact.
CompressionInstalled compression and contact pressureContact area and contact resistance change with compression.
Mating surfaceMetal, plated metal, conductive coating or another foamThe interface can dominate the measured contact resistance.
Cleaning and handlingSolvents, abrasion and handling cyclesSurface change must be tested, not assumed.

Forms and conversion

We supply the conductive grade as sheet, roll, slit strip, die-cut part, laminated sheet and adhesive-backed part. Common converted forms include tray liners, dividers, slot inserts, grounding pads, end cushions and contact strips. Die-cutting, CNC routing, lamination, slitting and adhesive backing are reviewed against the drawing, the base grade and the layer construction.

Tray, crate, divider and blister-tray pages are routes for individual review. Foam manufacture does not establish that every rigid crate or injection-moulded carrier is made in-house.

Typical routes, not approvals

Conductive IXPE is commonly evaluated for ESD trays and dividers, electronic chassis contact cushions, PCB and PCBA handling, battery-module contact parts and control-cabinet grounding paths. Each route has its own ESD plan, contact materials, cleanliness requirements and acceptance tests. The material grade does not approve the route; the customer’s ESD coordinator and the assembly owner remain responsible for the final approval.

Published IXPE base properties

Published factory data are grade- and method-specific. MD means machine direction; TD means transverse direction. Test-sheet values describe the material, not the finished assembly. On a small screen, scroll each table horizontally.

RatioDensity (kg/m³)Tensile MD/TD (MPa)Elongation MD/TD (%)Compression set (%) 23±2 °C, 22 hWater absorption (%)Thermal conductivity (W/m·K)
3×300±40≥1.6 / ≥1.4≥230 / ≥210≤2≤0.2≤0.095
5×200±30≥1.5 / ≥1.3≥220 / ≥200≤2≤0.2≤0.095
8×125±15≥1.0 / ≥0.9≥170 / ≥150≤3≤0.2≤0.084
10×100±10≥0.8 / ≥0.7≥150 / ≥130≤5≤0.2≤0.073
15×66.7±8≥0.6 / ≥0.5≥150 / ≥130≤7≤0.2≤0.065
20×50±6≥0.5 / ≥0.4≥150 / ≥130≤8≤0.3≤0.055
25×40±4≥0.4 / ≥0.3≥120 / ≥110≤9≤0.3≤0.049
30×33.3±3≥0.25 / ≥0.2≥120 / ≥110≤10≤0.4≤0.045
35×28.6±2≥0.2 / ≥0.15≥110 / ≥100≤11≤0.4≤0.040
40×26.8±3≥0.15 / ≥0.12≥110 / ≥100≤11≤0.4≤0.040

Test standards: density GB/T 6343 · tearing strength GB/T 10808 · tensile strength and elongation GB/T 6344 · water absorption GB/T 1034 (method 4) · thermal conductivity GB/T 10297 · compression set GB/T 6669 · dimensional change GB/T 8811. These are material tests; they do not certify a converted part or a package.

What the grade does not establish

Not EMI/RFI shielding. We do not publish shielding effectiveness in dB or by frequency. A conductive resistance range does not demonstrate shielding.

Not a dielectric rating. We do not publish breakdown voltage, comparative tracking index or dielectric strength. The foam must not be used as the insulation between a live conductor and a person or a grounded surface.

Not a cleanroom or cleanliness claim. We do not publish particle count, ionic contamination, outgassing or cleanroom class data. Where those requirements exist, they must be agreed and validated for the selected grade and the finished part.

Not a lifetime or humidity-independence promise. Resistance and contact resistance can change with humidity, temperature, cleaning, abrasion and handling. Define the conditioning, cleaning exposure and retest interval your programme requires.

Not food-contact or medical approval. We do not infer food-contact, medical or biocompatibility approval from the polymer or the cross-linking route.

Flame rating is material-level only. A flame-retardant grade can be supplied (LOI 27, GB 8410 A0, UL94 V2), but a material rating does not certify the finished part, the assembly or the end product.

Ordering, MOQ, lead time and samples

Standard rolls and sheets: MOQ 1,000 m². Custom parts: minimum quantity confirmed from the drawing. Standard lead time is 15–20 days from order confirmation; confirm the schedule for the selected grade and construction.

A4 material samples are free with shipping included. Machined samples, tooling and fixtures are quoted separately. Send the application, thickness, ratio or density, dimensions, quantity, resistance target, test method, contact face and working environment.

Bofeng Foam manufactures XPE, IXPE and IXPP in Zhuhai. Existing grade specifications and available reports can be requested. ISO 9001 and ISO 14001 are management-system certifications, not product approvals.

FAQ

Is conductive foam the same as shielding foam?

No. Conductive describes a resistance range. Shielding describes attenuation of an electromagnetic field and is measured in dB by frequency. We do not publish a shielding figure, and a conductive resistance reading does not prove shielding.

Which grade should I use, 10³ or 10⁶?

Choose by function. Use the conductive range when charge must be carried to a ground or a contact path is required; use the anti-static (dissipative) range when the aim is to avoid charge build-up without a low-resistance connection. Confirm the target with your ESD control plan.

Does compression change the resistance?

It can change the contact resistance and the measured result. Define the installed compression and test the actual contact face and mating surface. A material data sheet alone does not predict the installed joint.

Can you die-cut a thin conductive pad?

Yes. IXPE single-layer thickness starts at 0.1 mm. The practical minimum depends on the part shape, the die, the adhesive and the handling requirement.

Related material and application pages