A charging pile used to be an electrical cabinet with a fan and a modest power module inside it. The foam was ordinary transit cushioning plus a dust strip on the door. A current DC cabinet is a different object: the module often sits on a liquid-cooled cold plate, the power per litre is several times higher, the enclosure is closed against weather, and the unit is expected to repeat that duty cycle every day for years. The foam has not become more important in that design, but the questions asked of it have become more specific, and several of them a foam supplier cannot answer at all.
This page covers the three places foam actually appears around a charging power module, what each of those places is accepted by, and where the material stops. There is a fourth position that this article deliberately does not count as a seat — the bolted joint between the module and its bracket — and it gets its own section below, because it is the position where a pad is most easily mistaken for a structural part. The general case for equipment that is not charging-specific — cushioning, sealing, sound and vibration in electromechanical machinery — is on our electromechanical selection guide; this article is the charging-pile part of that picture.
1. Why a current charging pile puts foam in a harder place
Three changes in cabinet design move the foam requirements, and none of them is about the foam itself.
The module runs hotter at its surface. When a module is cooled through a cold plate, the heat leaves through one face and the rest of the housing becomes a warm structure with a defined interface temperature. Foam pressed against that structure sees a temperature that comes from the coolant loop and the ambient, not from the datasheet of the foam. The duty cycle adds a daily swing on top of it.
The cabinet is closed. A closed cabinet with a filtered air path means the foam strip on a panel is part of a dust strategy, not a door decoration. It also means condensation has nowhere to go, and foam is not a desiccant.
The internal clearances are designed, not assumed. In a 400 V or 800 V architecture, the distance between a live busbar and a metal housing is a design value agreed between the module maker and the cabinet maker. Foam may sit in that gap as a mechanical spacer. It does not create the clearance, and it does not certify it.
Each of these changes pushes the same way: the foam accepts a narrower role, with a tolerance and a temperature attached to it.
2. What each seat in the cabinet is accepted by
The word "cushion" covers three different jobs in one cabinet. They are accepted by three different tests, and a material datasheet answers none of them directly.
One thing belongs in front of that table: more than one foam family sits in a charging cabinet, and they are not substitutes. Open-cell melamine foam is the one sold for cabinet lining, module wrap and noise control — light, flame-retardant and acoustically effective, and open-cell, so it is not a water-resistant part. EPDM and silicone sponge are what gasket makers specify for the enclosure seal. Closed-cell PE, the material in this article, is specified where the reason is water uptake, a die-cut tolerance part, a baffle or a bumper. A buyer comparing quotes across those three families is comparing three different jobs.
| Location | Job on the drawing | What accepts it | Who runs the test |
|---|---|---|---|
| Transit cushion inside the module carton | Limit shock to the module on drop | A pack-level drop or shock test at the agreed level, module undamaged and still within its functional check | Module maker or packing lab |
| Strip between the cabinet panel and the frame | Reduce the dust path into the electronics compartment | A cabinet ingress test, if an IP class is required | Cabinet maker |
| Spacer between the module housing and the enclosure wall | Hold an agreed mechanical clearance | Dimensional inspection of the assembled unit | Design authority, normally the module maker |
Notice that the last column never says "foam supplier". The material supplies a behaviour; the acceptance happens on the module or on the cabinet. A foam drawing that quotes only density and thickness has left the actual requirement — load, compression, temperature, tolerance — undefined.
3. The heat path belongs to the pad, not the foam
Cross-linked PE foam is an insulator. Its thermal conductivity in our published data runs from 0.040 to 0.095 W/m·K depending on expansion ratio, and it gets worse as the foam gets lighter. A thermal gap pad, a gap filler or a phase-change material works in a different range and through a different mechanism: those parts are designed to carry heat from a heat source to a sink, and their datasheets are written in thermal resistance, not in compression.
If a module design needs heat to leave through an interface, foam is the wrong material for that interface. What foam can do next to it is hold position: keep a cable or a connector from touching the hot housing, pad the space where the cold plate and the enclosure meet so that the two do not rub, and fill a non-thermal gap where nothing is being cooled.
It is worth being explicit in the drawing, because "thermal foam" is a phrase that appears in purchasing documents and means nothing precise. If the requirement is thermal resistance, name the interface material. If the requirement is mechanical, name the foam and write the compression.
4. The bolted joint: why it is not one of the seats
This is the position deliberately left out of the table. A module is bolted to a bracket, and the bracket is welded to a cabinet frame. Two painted steel surfaces under a bolt do not sit perfectly flat, and the module sees vibration in transport and in service. What shows up is visible at the joint: paint rubbed through at the high spots, a polished witness mark on the housing, and a bracket torque that has to be re-checked at service intervals.
If a pad is put in that gap, it does three useful things. It takes up the tolerance between the bracket and the module face. It separates the two painted surfaces so that they are not metal to metal at the high spots. And it adds a little damping, which is worth having when the pad is thick enough for it to matter.
What it does not do is hold the joint together, and there are two separate reasons for saying so. The first is data: we publish no force–displacement curve for a compressed part, so a pad cannot be designed as a load path from a current datasheet alone. The second is mechanical: a soft layer under a clamped joint lowers the stiffness of that joint, so a pad is not the remedy for a joint that moves. If relative movement is the problem, the answers are the clamp load, a hard spacer, a thread-locking feature, or a design that does not put a bolted joint there at all.
This should also be kept separate from a problem with a similar name. Relative movement at an electrical contact is a well-known cause of rising contact resistance: the plating wears, the base metal oxidises, and the resistance climbs before anything looks broken. That failure belongs to the terminal, its plating and its contact load. A foam pad next to the connector changes none of those three, and a supplier who offers foam as the fix for it is answering the wrong question. On bolted power connectors the same literature traces the chain back to a cracked spring washer and lost clamping force, which is why maintaining clamp force — not adding a soft layer — is the protective measure.
5. Daily thermal cycling: compression set is the number that decides
The most common field failure of a foam pad in a cabinet is not tearing and not melting. It is that the pad gradually stops pushing back. Every thermal cycle compresses and releases it, and a closed-cell PE foam keeps a small permanent deformation. Over months the gap opens, the pad no longer touches both surfaces, and the separating job is gone even though the foam still looks intact.
The published number that speaks to this is compression set, measured at 23±2 °C for 22 hours. It is a material value, not a life prediction, and it is the only one we publish. There is no hot-set or cycled-set figure in our data. If the application needs one, it is a test to be run on the part and written into the qualification plan — not something to be read across from the room-temperature number.
Before any of this goes onto a drawing, make one comparison. The usual test condition for a gasket material is 70 °C for 22 hours; our figure is measured at 23±2 °C for 22 hours. Both are legitimate tests and they are not the same number — a compression set measured hot reads higher. Put the test condition next to the value whenever two grades are compared, or the comparison is between a room-temperature result and a hot one.
| Ratio and density | Compression set, 23±2 °C, 22 h | Thermal conductivity |
|---|---|---|
| 3× (300 kg/m³) | ≤2% | ≤0.095 W/m·K |
| 10× (100 kg/m³) | ≤5% | ≤0.073 W/m·K |
| 20× (50 kg/m³) | ≤8% | ≤0.055 W/m·K |
| 30× (33.3 kg/m³) | ≤10% | ≤0.045 W/m·K |
| 40× (26.8 kg/m³) | ≤11% | ≤0.040 W/m·K |
Two cautions follow from the way that table is built. First, the test is 22 hours at room temperature, while the cabinet sees thousands of hours at its operating temperature; a low compression set at 23 °C is a starting point, not a promise about the field. Second, the lighter the foam, the larger the set. A 40× foam chosen to save weight in the pad is the grade most likely to loosen first, and it is also the grade with the lowest force at a given compression, so the pad has to be thicker to do the same job.
Heat ageing has its own number. At 70±2 °C for 22 hours the dimensional change of XPE and IXPE is a shrinkage of no more than about 4% transverse and 6% machine direction up to 15×, and up to 6% and 8% at 20× and above. A pad that is 6 mm thick and shrinks 3% loses nearly 0.2 mm of a 0.2 mm interference in one ageing cycle. That is the mechanism by which a correctly sized pad becomes loose without any visible damage.
6. Airflow, dust and condensation: a separator, not a seal
IXPE is closed-cell and takes up very little water — 0.2% to 0.4% by the published test, depending on ratio. That is why it is used as a strip between a panel and a frame where the goal is to reduce the dust path into the electronics compartment.
It is worth being exact about what that strip does, because two different parts in a cabinet are both called "dust foam". The part at the air intake is a filter: an open-cell foam or a filter mat held in a frame, whose job is to trap particles while air passes through it. A closed-cell PE strip cannot do that job at all — air does not pass through it. Its job is a baffle: it forces the air to turn a corner and closes the straight path that a dust-laden draught would otherwise take. A baffle with a gap at one end is not a barrier, so the gap is the item to specify, and it matters more than the material.
It is not a seal, and the cabinet's IP class is not something a foam datasheet can carry. Ingress protection is a property of the assembled enclosure: strip geometry, compression, frame flatness, fastener spacing, adhesive and closing force. If an IP class is in the specification, the cabinet is what gets tested, and the foam drawing should say "component of the sealing system", not "IP54 seal".
Condensation is the harder half of the same problem. A closed cabinet that heats during the day and cools at night will move moisture to its coldest internal surface, and foam wrapped on a cold part can hold that moisture against it. A foam that resists water uptake slows the process; it does not solve it. The solution belongs to the enclosure designer — a breather, a heater, a coating or a drainage path — and a foam supplier who promises to solve condensation is overreaching.
7. Clearance, creepage and the spacer question
In a high-voltage cabinet, foam sometimes sits between a module housing and an enclosure wall, holding a mechanical gap. This is a legitimate use, and it needs a clear boundary in the drawing.
The foam holds a distance. It does not provide electrical insulation as a rated function. We do not publish dielectric strength or breakdown voltage for these materials, and they should not be used as the dielectric in a design that depends on the foam to keep a live part away from grounded metal. The distance itself comes from the applicable standard and from the module maker's design; the foam's job is to make sure that distance survives assembly, transport and service.
There is also a materials point that belongs in the same conversation. A foam spacer that compresses under assembly load changes the geometry it was meant to hold. If the clearance is critical, the spacer should be specified with a compression at the assembly load, or made from a grade with a higher compression force, or replaced by a hard part and the foam used only as a soft interface.
8. Specification checklist for a charging power module
A drawing that answers these lines can be quoted and checked. A drawing that answers fewer of them will be re-opened during first article inspection.
- Seat: which of the three positions, and one function per line item.
- Load: the compression force expected at the installed thickness, and whether the pad carries the bolt load or only fills.
- Compression: the installed thickness and the free thickness, so the working ratio is unambiguous.
- Temperature at the pad, over the duty cycle, including the hottest abnormal case the cabinet must survive.
- Flame requirement, stated at material level or cabinet level, with the standard named.
- Dust or ingress role, and whether an enclosure test is required.
- Adhesive: substrate, service temperature, and whether the part is taped, clipped or loose.
- Static requirement, if any: conductive or anti-static grade, the target range, and the method agreed for measuring it.
- Part form: die-cut, CNC-routed, laminated or slit, with the tolerance on each dimension.
- Annual quantity and pack format.
9. What Bofeng Foam will and will not put on the drawing
On the material side we can state the grade, the expansion ratio, the density, the compression set, thermal conductivity, water uptake and the dimensional change at 70 °C, all from our published data. The parts described above are made from IXPE foam or IXPP, and they are listed on the electromechanical equipment foam application page. We can supply a flame-retardant grade with LOI 27, GB 8410 A0 and UL94 V2, and conductive or anti-static grades in the ranges 10³–10⁶ Ω and 10⁶–10⁹ Ω; the measurement method for those resistance figures (surface or volume) has to be agreed per project, because both are used in the industry and they are not interchangeable. We can die-cut, CNC-route, laminate, slit and apply adhesive, and we work from a drawing to a first article.
What we will not do is sign a line we cannot support. No dielectric strength, breakdown voltage or insulation rating. No EMI or RFI shielding figure in dB. No IP class for a foam strip. No particle, outgassing or cleanroom classification. No vibration transmissibility for a loaded pad. No service-life figure in years. No claim of blocking thermal runaway, and no UN38.3, UL 2580 or IEC 62619 approval. Higher UL94 vertical burn ratings than V2 are not offered; our flame grades are LOI 27, GB 8410 A0 and UL94 V2, plus UL94 HF-1 and GB8624-B1 on request. Those four decisions belong to the module and cabinet makers and to the test house they choose.
The company has been producing foam since 2011, with five production lines and an annual capacity of 5,000 tonnes. Standard material is quoted at a minimum of 1,000 m²; custom die-cut parts are quoted from a drawing. Lead time is 15–20 days after drawing approval, and an A4 sample is free with the freight included. Send the drawing with the ten items above, and the reply will be a grade, a thickness, a compression and a price — or a question about the line that is still undefined.